Introduction of the metal and oxide powder made by various composition methods
Shape control of Ag particle by wet method
-
Silver nanoparticles
-
Silver submicron particles
-
Silver board-formed particles
-
Silver string-formed particles
Shape control of WO3 particles by the wet method
-
Board-formed particles
-
Needle-formed particles
-
Granular particles
Catalytic needle-formed nanoparticles by wet method
-
- MO3 needle-formed nanoparticles
- Diameter: 20nmlength: 100-200nm
-
- WO3 needle-formed nanoparticles
- Diameter: 10nmlength: 100-200nm
Creation of nanoparticles by various wet processes
ZnO nanoparticles
Average size 5nm
The reason why the liquid of left lower picture is transparent is ZnO nanoparticles are distributed in ethanol.
It is not possible to measure the density because it vaporizes with ethanol.
We cannot manufacture in large quantities now, because we only study with small quantity.
An example of the porous active material particle
Sn porous materials as cathode materials of next-generation
Nanoporous micron Silica powder
- 1. Content of Silica
- more than 98% including K, Ca, and Al in small quantities
- 2. Softening point
- 1,000 degrees Celsius or more
almost same as the point of quartz because of purity of Silica
- 3. Particle size
- 5-30 microns
- 4. Primary particle size
- 50-100nm
- 5. BET
- 30-50m2/g
- 6. Property
- Nanoporous particle